Effect of Sintering Time on the Densification, Microstructure, Weight Loss and Tensile Properties of a Powder Metallurgical Fe-Mn-Si Alloy

preprint OA: closed
View at publisher

Abstract

This work investigated the isothermal holding time dependence of the densification, microstructure, weight loss and tensile properties of Fe-Mn-Si powder compacts. Elemental Fe, Mn and Si powder mixtures with a nominal composition of Fe-28Mn-3Si (in weight percent) were ball milled for 5h and subsequently pressed under a uniaxial pressure of 400 MPa. The compacted Fe-Mn-Si powder mixtures were sintered at 1200 ℃ for 0, 1, 2 and 3 h, respectively. In general, the density, weight loss and tensile properties increased with the increase of isothermal holding time. A significant increase in density, weight loss and tensile properties occurred in the compacts isothermally holding for 1 h, as compared to those with no isothermal holding. However, further extension of isothermal holding time (2 and 3 h) only played a limited role in promoting the density and tensile properties. The weight loss of the sintered compacts was mianly caused by the sublimation of Mn in Mn depletion region on the surface layer of the sintered Fe-Mn-Si compacts. The length of the Mn depletion region increased as isothermal holding time increased. A single α-Fe phase was detected on the surface of all the sintered compacts, and the locations beyond the Mn depletion region were comprised of a dual dominant γ-austenite and minor ε-martensite.

My notes (saved in your browser only)

Citation neighborhood (no data yet)

We don't have any in-corpus citations linked to this paper yet. The paper's references may be in our DB but unresolved to ``paper_id`` (resolution happens at ingest when the cited DOI matches a row we already have). Run the cross-source citation reconcile pass to retry.

Source provenance

europepmc
last seen: 2026-05-19T01:45:01.086888+00:00