Background: For the treatment of bone defects, biodegradable compressive biomaterials are needed as a substitute, which degrade at the same rate as the bone regenerates. In this study, the compressive strength of CPC ceramics (with a layer thickness of more than 12 layers) should be compared with sintered ceramics. Methods: Round scaffolds with 20, 25, 30 and 45 layers were 3D printed the 3D Bioplotter, solidified in a water-saturated atmosphere for 3 days and then tested for compressive strength together with a sintered ceramic using a Zwick universal testing machine. Results: The 3D printed scaffolds are more compressive at 41.56 ± 7.12 MPa than the sintered ceramic at 24.16 ± 4.44. Conclusions: The round geometry sintered ceramics approach or exceed the upper limit of the compressive strength of cancellous bone in the direction of compacta (depending on the author).
My notes (saved in your browser only)
Citation neighborhood (no data yet)
We don't have any in-corpus citations linked to this paper yet. The paper's references may be in our DB but unresolved to ``paper_id`` (resolution happens at ingest when the cited DOI matches a row we already have). Run the cross-source citation reconcile pass to retry.
Source provenance
- europepmc
- last seen: 2026-05-19T01:45:01.086888+00:00
- unpaywall
- last seen: 2026-06-06T02:00:05.402940+00:00
License: CC-BY-4.0