CVDを利用した炭素/阿蘇黄土複合体の合成
article
OA: closed
CC0
Abstract
Carbon/limonite composite was synthesized through chemical vapor deposition of CH4 with a help of catalysis of limonite. The limonite was heat-treated at 600℃ 5 h in air before the chemical vapor deposition in order to remove impurities. When synthesis temperature was over 889℃, carbon was deposited on the limonite. Moreover, when synthesis temperature was over 1025℃, soot deposition was observed on the inner wall of reaction tube. The amount of the deposits increased with increasing synthesis temperature and time. The obtained composite was attracted by magnet.
My notes (saved in your browser only)
Citation neighborhood (no data yet)
We don't have any in-corpus citations linked to this paper yet. The paper's references may be in our DB but unresolved to ``paper_id`` (resolution happens at ingest when the cited DOI matches a row we already have). Run the cross-source citation reconcile pass to retry.
Source provenance
- openalex
- last seen: 2026-05-10T10:56:23.340211+00:00
License: CC0
· commercial use OK